Polyolefin elastomer nylon toughness modification improve material impact strength
Classification: | Chemical Auxiliary Agent |
Place of Origin: | Shanghai, China |
Type: | Carbon Black |
Usage: | Plastic Auxiliary Agents, Widely |
Test conditions: | Room temperature 230℃/2.16KG |
Typical values: | ASTM D792 ASTM D1238 |
Test method: | Infrared absorption spectrometry |
Density: | 0.868 g/cm3 |
PDF |
|
Product Details
Classification | Chemical Auxiliary Agent |
Place of Origin | Shanghai, China |
Type | Carbon Black |
Usage | Plastic Auxiliary Agents, Widely |
Test conditions | Room temperature 230℃/2.16KG |
Typical values | ASTM D792 ASTM D1238 |
Test method | Infrared absorption spectrometry |
Density | 0.868 g/cm3 |
Melting index | 1.0g/10min |
Grafting ratio | 1.0% |
Color | White |
Shape | Granules |
Material | Polyolefin |